Constarium
← Search

Structure · dataset · 2017

Effects of Rolling Deformation and Annealing Treatment on Damping Capacity of 1200 Aluminium Alloy

Listed in DataCite

Annealing treatment is an important step of rolling deformation that contributes to microstructural evolution and leads to the significant changes in damping capacity.

Description

Damping capacities were analyzed in the parallel to rolling direction at 1 and 10 Hz respectively. It was found that severe plastic deformation at 40 percent reduction has lower damping capacity compared to that of 30 percent and 20 percent reductions respectively.

The microstructural results show that the grains of as rolled alloys were changed to almost equiaxed structures after a rolling reduction at 40 percent reduction. Full paper can be downloaded via below arXiv URL.

Links

Topics

Stated by source
Materials engineering
Inferred from text
Materials engineering 69%

Related

Provenance · 1 source records, 10 field assertions
SourceKeyLast seenRaw
DataCite10.6084/m9.figshare.4910708.v212 d agoJSON v1
FieldAssertionExtractorEvidence
access_levelsource · DataCiteconnector:datacite@1.0.0/data/attributes/rightsList
byte_sizesource · DataCiteconnector:datacite@1.0.0
concepts[field].anzsrc:group:4016enrichment · DataCitetaxonomy-embedding@1.1.0title+keywords+description (69%)
concepts[field].fos:materials-engineeringsource · DataCiteconnector:datacite@1.0.0
created_datesource · DataCiteconnector:datacite@1.0.0
descriptionsource · DataCiteconnector:datacite@1.0.0/data/attributes/descriptions
licensesource · DataCiteconnector:datacite@1.0.0/data/attributes/rightsList
publication_datesource · DataCiteconnector:datacite@1.0.0/data/attributes/dates
titlesource · DataCiteconnector:datacite@1.0.0/data/attributes/titles/0/title
updated_datesource · DataCiteconnector:datacite@1.0.0